供应 Luran® S KR 2858 G3 | ASA-GF15 | Styrolution
Rheological properties | Value | Unit | Test Standard |
CAMPUS/ISO Data |
Melt volume-flow rate (MVR) | 5 | cm³/10min | ISO 1133 |
Temperature | 220 | °C | ISO 1133 |
Load | 10 | kg | ISO 1133 |
Mechanical properties | Value | Unit | Test Standard |
CAMPUS/ISO Data |
Tensile Modulus | 6600 | MPa | ISO 527-1/-2 |
Stress at break | 110 | MPa | ISO 527-1/-2 |
Strain at break | 2.5 | % | ISO 527-1/-2 |
Charpy impact strength (+23°C) | 28 | kJ/m² | ISO 179/1eU |
Charpy impact strength (-30°C) | 17 | kJ/m² | ISO 179/1eU |
Charpy notched impact strength (+23°C) | 7 | kJ/m² | ISO 179/1eA |
Charpy notched impact strength (-30°C) | 6 | kJ/m² | ISO 179/1eA |
Thermal properties | Value | Unit | Test Standard |
CAMPUS/ISO Data |
Temp. of deflection under load (1.80 MPa) | 110 | °C | ISO 75-1/-2 |
Temp. of deflection under load (0.45 MPa) | 115 | °C | ISO 75-1/-2 |
Vicat softening temperature (50°C/h 50N) | 115 | °C | ISO 306 |
Coeff. of linear therm. expansion (parallel) | 30 | E-6/K | ISO 11359-1/-2 |
Burning Behav. at 1.5 mm nom. thickn. | HB | class | IEC 60695-11-10 |
Thickness tested | 1.6 | mm | IEC 60695-11-10 |
Burning Behav. at thickness h | HB | class | IEC 60695-11-10 |
Thickness tested | 0.8 | mm | IEC 60695-11-10 |
Other properties | Value | Unit | Test Standard |
CAMPUS/ISO Data |
Water absorption | 1.42 | % | Sim. to ISO 62 |
Humidity absorption | 0.3 | % | Sim. to ISO 62 |
Density | 1180 | kg/m³ | ISO 1183 |
Test specimen production | Value | Unit | Test Standard |
CAMPUS/ISO Data |
Injection Molding, melt temperature | 250 | °C | ISO 294 |
Injection Molding, mold temperature | 60 | °C | ISO 10724 |
Injection Molding, injection velocity | 200 | mm/s | ISO 294 |