供应ASA 777K 德国巴斯夫
Luran® S 777 K | ASA | Styrolution
易流动注射成型具有良好的韧性和耐热变形性
Rheological properties | Value | Unit | Test Standard |
CAMPUS/ISO Data |
Melt volume-flow rate (MVR) | 15 | cm³/10min | ISO 1133 |
Temperature | 220 | °C | ISO 1133 |
Load | 10 | kg | ISO 1133 |
Molding shrinkage (parallel) | 0.5 | % | ISO 294-4, 2577 |
Molding shrinkage (normal) | 0.9 | % | ISO 294-4, 2577 |
Mechanical properties | Value | Unit | Test Standard |
CAMPUS/ISO Data |
Tensile Modulus | 2300 | MPa | ISO 527-1/-2 |
Yield stress | 48 | MPa | ISO 527-1/-2 |
Yield strain | 3.3 | % | ISO 527-1/-2 |
Nominal strain at break | 9 | % | ISO 527-1/-2 |
Tensile creep modulus (1h) | 1850 | MPa | ISO 899-1 |
Tensile creep modulus (1000h) | 1400 | MPa | ISO 899-1 |
Charpy impact strength (+23°C) | 250 | kJ/m² | ISO 179/1eU |
Charpy impact strength (-30°C) | 90 | kJ/m² | ISO 179/1eU |
Charpy notched impact strength (+23°C) | 17 | kJ/m² | ISO 179/1eA |
Charpy notched impact strength (-30°C) | 4 | kJ/m² | ISO 179/1eA |
Thermal properties | Value | Unit | Test Standard |
CAMPUS/ISO Data |
Temp. of deflection under load (1.80 MPa) | 97 | °C | ISO 75-1/-2 |
Temp. of deflection under load (0.45 MPa) | 101 | °C | ISO 75-1/-2 |
Vicat softening temperature (50°C/h 50N) | 97 | °C | ISO 306 |
Coeff. of linear therm. expansion (parallel) | 95 | E-6/K | ISO 11359-1/-2 |
Burning Behav. at 1.5 mm nom. thickn. | HB | class | IEC 60695-11-10 |
Thickness tested | 1.6 | mm | IEC 60695-11-10 |
UL recognition | UL | - | - |
Burning Behav. at thickness h | HB | class | IEC 60695-11-10 |
Thickness tested | 0.8 | mm | IEC 60695-11-10 |
UL recognition | UL | - | - |
Oxygen index | 19 | % | ISO 4589-1/-2 |
Electrical properties | Value | Unit | Test Standard |
CAMPUS/ISO Data |
Relative permittivity (100Hz) | 3.7 | - | IEC 60250 |
Relative permittivity (1MHz) | 3.4 | - | IEC 60250 |
Dissipation factor (100Hz) | 110 | E-4 | IEC 60250 |
Dissipation factor (1MHz) | 240 | E-4 | IEC 60250 |
Volume resistivity | 1E12 | Ohm*m | IEC 60093 |
Surface resistivity | 1E13 | Ohm | IEC 60093 |
Electric strength | 35 | kV/mm | IEC 60243-1 |
Comparative tracking index | 600 | - | IEC 60112 |
Other properties | Value | Unit | Test Standard |
CAMPUS/ISO Data |
Water absorption | 1.65 | % | Sim. to ISO 62 |
Humidity absorption | 0.35 | % | Sim. to ISO 62 |
Density | 1070 | kg/m³ | ISO 1183 |
Rheological calculation properties | Value | Unit | Test Standard |
CAMPUS/ISO Data |
Thermal conductivity of melt | 0.16 | W/(m K) | - |
Spec. heat capacity melt | 1860 | J/(kg K) | - |
Ejection temperature | 95 | °C | - |
Test specimen production | Value | Unit | Test Standard |
CAMPUS/ISO Data |
Injection Molding, melt temperature | 250 | °C | ISO 294 |
Injection Molding, mold temperature | 60 | °C | ISO 10724 |
Injection Molding, injection velocity | 200 | mm/s | ISO 294 |